Home > Products > Packaging , Printing & Paper > Packaging Materials > Plastic Packaging Materials

BOPP Thermal Laminating Film 1BOPP Thermal Laminating Film 2BOPP Thermal Laminating Film 3BOPP Thermal Laminating Film 4
  • BOPP Thermal Laminating Film 1
  • BOPP Thermal Laminating Film 2
  • BOPP Thermal Laminating Film 3
  • BOPP Thermal Laminating Film 4

BOPP Thermal Laminating Film

Model:APPEXL-G20
Brand:APPEXL
Origin:Made In China
Category:Packaging , Printing & Paper / Packaging Materials / Plastic Packaging Materials
Label:thermal film , bopp thermal film , bopp lamination film
Price: US $2940 / MT
Min. Order:2 MT
Inquire Now Add to Basket

Member Information

Detail

Product Description

Professional producer for BOPP Thermal Laminating Film.
Typical thickness: Glossy 25mic(12BOPP+13EVA) and Matte 27mic(15BOPP+12EVA). Single or double corona treatment.
20 days delivery of a 40feet container!

As an environmental friendly product, BOPP Thermal Laminating Film features as below:
#1 Healthy Lamination Process
It is non-hazardous to health and safe to use as being without toxic gases nor volatile content.
It is also safe during laminating process due to no solvent-based adhesive used.
#2 Easy Operation
It requires no action of using and blending the rubber, solvent, diluent and so on which is much easier during handling and cost-saved compared with the old way.
No special technique required, just laminate when the temperature gets adequate.
It is recommended to laminate the film with dry laminator. Just small adjustment to the machine needed if the film is laminated with wet laminator...
#3 High Efficiency and Energy-saving
Production cost is substantially reduced due to no wastage of film generated, no mixing of adhesive, no coating and drying processes, nor UV heating lamp required.
#4 Outstanding Function and Effect
It enhances the finished item's value through high transparency and super luster finish.
Preventing lamination from being pressed, bubbled and desquamated.
Protected from harmful substances and water-proof, ensuring a long life storage for the printings.
Particularly, matte BOPP Thermal Lamination Film is good for spot UV and hot stamping.

APPLIED TO
Books, Posters, Presentation Folders, Labels, Shopping Bag, POP Signs, Document, Book Covers, ID Cards, License, Passports, Antigraffiti, Boardmaking,
Write on/wipe off Calendars, Photographs, Albums ect.
Outside coating for wrapping box or bag for food, medicine, cosmetic, gift, liquor etc.
Drawing paper, documents, advertisement, digital printing, show board, etc.

PRODUCT        TECHNICAL        PARAMETER
THICKNESS (micron) BOPP (BASE) 12 micron 12 micron 15 micron 15 micron 15 micron
EVA (GLUE) 8 micron 13 micron 10 micron 12 micron 13 micron
TOTAL 20 micron 25 micron 25 micron 27 micron 28 micron
TYPES Glossy
Matte    
Customized thickness-combination Available
Yield/Ration Glossy 54.230m2/kg 44.215m2/kg 43.526m2/kg 40.212m2/kg 38.655m2/kg
Matte     44.843m2/kg 41.344m2/kg 37.174m2/kg
THICKNESS TOLERANCE ±1.5um
WIDTH RANGE per roll 300mm---1600mm   (±5mm)
LENGTH RANGE per roll 2000m, 3000m, 4000m   (±3%)   
PAPER CORE (INNER DIA.) 25.4mm (1");   76mm (3")
CONNECTOR/BONDING ≤ 1
CORONA TREATMENT SIDE one side or both sides
SUR. TENSION (AFT. CORONA) ≥ 42dyne
APPLICATION MANUAL
COMPOUND TEMPERATURE 85--110C        (185-230F)
COMPOUND PRESSURE 10--18mpa
COMPOUND SPEED 10--60m/min
APPLICATION GUIDANCE
* Better to be used in dry laminator. Small adjustment to the machine required when used in wet laminator.
* Normal process temperature is 90C-105C (203F - 221F), roller pressure and temperature vary from   
  different types of paper, ink and machines.
* When using the film for the first time or doing other treatment, please try a small volume before massive 
   laminating.
* Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture
  or powder.
* Make sure to put the material in place with low temperature and dry.
* The following situation will affect the final quality of the film during lamination.  
a. metal ink  
b. ink containing too much wax, dried oil, adhesive, silicon additive and so on.   
c. too much thick ink                                d. ink completely undried  yet   
e. too much humid paper sheet             f. too much powder on the surface  
 



Payment Terms:TT/LC

Product Image

BOPP Thermal Laminating Film 1
Img 1
BOPP Thermal Laminating Film 2
Img 2
BOPP Thermal Laminating Film 3
Img 3
BOPP Thermal Laminating Film 4
Img 4

Send Inquiry to this Member

Authentic Plastic Packing Enterprise Xiamen Limited

Neikeng Industrial Zone,Huli District,Xiamen China

Phone:
86-592-5257614
Fax:
86-592-5257624
Contact:
Stewart Ren (Sales)
Mobile:
+86-592-5257614

Related Products of this Company

This member assumes full responsibility for the content of this listing. DIYTrade accepts no responsibility whatsoever in respect of such content.
To report fraudulent or illegal content, please click here.

China Suppliers Quick Searching:

Plastic Packaging Materials Made In China Products

,  

Plastic Packaging Materials China Suppliers and China Manufacturers