Alloy 904L tubing and pipe/ Aleación de tubo y tubería 904L
Product Description
Physical Properties of Super Austenitic 904L Alloys in the Annealed Condition at -20°F to +100°F
|
|
|
Tensile Strength |
Yield Strength |
|
|
|
|
|
|
Alloy |
UNS Designation |
Spec. |
psi |
MPa |
ksi |
psi |
MPa |
ksi |
Elongation in 2 in. (min.) % |
Grain Size Req. |
Max. Hardness |
Modulus of Elasticity (x106psi) |
Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) |
Thermal Conductivity (BTU-in/ ft2-h-°F) |
904L |
N08904 |
A249, A312 |
71,000 |
490 |
71 |
31,000 |
215 |
31 |
35 |
— |
90 Rb |
28.0 |
8.5 |
79 |
904L |
N08904 |
B673, B674 |
71,000 |
490 |
71 |
31,000 |
215 |
31 |
35 |
— |
— |
— |
8.5 |
79 |
Composition of Super Austenitic 904L tubing and pipe
Grade |
904L |
UNS Designation |
N08904 |
Nickel (Ni) |
23.0 – 28.0 |
Chromium (Cr) |
19.0 – 23.0 |
Iron (Fe) |
Bal. |
Molybdenum (Mo) |
4.0 – 5.0 |
Titanium (Ti) Max. |
— |
Aluminum (Al) Max. |
— |
Cobalt (Co) Max. |
— |
Tungsten (W) |
— |
Vanadium (V) Max. |
— |
Copper (Cu) Max. |
1.00 – 2.00 |
Manganese (Mn) Max. |
2.00 |
Niobium (Nb) plus Tantalum |
— |
Carbon (C) Max. |
0.020 |
Nitrogen (N) Max. |
0.10 |
Silicon (Si) Max. |
1.00 |
Sulphur (S) Max. |
0.035 |
Phosphorous (P) Max. |
0.045 |
Other Elements |
— |
Super Austenitic 904L Product Range
Alloy |
UNS Designation |
Werkstoff NR. |
Specifications* |
904L |
N08904 |
1.4539 |
A269, A/SA249, B/SB674, A/SA312, B/SB673
|
Product Image
Img 1
Send Inquiry to this Member
Related Products of this Company
This member assumes full responsibility for the content of this listing. DIYTrade accepts no responsibility whatsoever in respect of such content.
To report fraudulent or illegal content, please
click here.
China Suppliers Quick Searching:
,