(1) Silicon mold preheating: heat the silicon mold to 60-70℃, low mold temperature will cause the solidification incompletely and the bad physical property. Mold temperature is directly correlated with the size precision of the part.
(2) Casting material debubbling: respectively debubble the A and B liquid material in the vacuum tank for over 30 minutes.
(3) Injection molding: place the A liquid container and B liquid container in the vacuum tank. Stir the B liquid to debubble it for 5-10 minutes, pour A liquid to B liquid and stir them , then inject the mixed A and B liquid to the silicon mold instantly. Resume atmosphere pressure of the vacuum tank within 1 minute from the beginning of the injection molding.
(4) Solidification: can release the mold after 30-60 minutes solidification in the 60-70 ℃ thermo tanks. If necessary, it can take the second solidification for 2-3 hours in the 70-80 ℃ thermo tanks.
Main technical specification:
Applicable mold: make the soft silicon mold for the need of building prototype; the silicon mold life is 10-20 times.
Casting material: PU. The used materials include Japan HEI-CAST and PELNOX、France AXSON.
Material physical property: similar ABS、similar PP、similar PC、similar PMMA (transparent) 、similar rubber (40-90 shofd D) 、high-temp resistance (150 ℃) 、fireproof material, etc.
General operation time: 1-4 hours/pc, 4-8 hours/pc (big size)
Molding precision: ±0.15mm/100mm
Molding thickness: Min. 0.5mm, favor 1.5-3.0mm
Payment Terms: | TT/ western union |
| |
Product Image
Send Inquiry to this Member
Related Products of this Company
This member assumes full responsibility for the content of this listing. DIYTrade accepts no responsibility whatsoever in respect of such content.
To report fraudulent or illegal content, please
click here.
China Suppliers Quick Searching:
,